422 Stainless Steel Bar - AMS 5655


Alloy 422 stainless bar is a hardenable, martensitic stainless steel designed for service temperatures as high as 1200 F. This grade develops high mechanical properties via heat treatment and offers good scaling and oxidation resistance.  Typical applications have included buckets and blades in steam turbines, high temperature bolting and valve and valve trim.

Standard Inventory Specifications

  • UNS S42200
  • AMS 5655
  • ASTM A 176
  • ASTM A 565
  • AMSE SA 176
  • B50A951 A1
  • B50A951 A2
  • AISI 636

Common Trade Names

  • 422 stainless
  • Alloy 422
  • 422

Industry Applications of Alloy 422 Stainless Steel

  • Power Generation 

Inventory Size Range

  • Bar : 0.500" - 13.000"
  • Standard Inventory Lengths: 10-12 feet rl's.

The technical data provided is for information only and not for design purposes. It is not warranted or guaranteed.

Chemical Composition of 422 Stainless Steel

Element

Percent by Weight

Carbon

0.20 – 0.25%

Chromium

11.50 – 13.50%

Phosphorus

0.040% max      

Molybdenum

0.75 – 1.25%

Sulfur

0.030% max      

Tungsten

0.75 -  1.25%

Silicon

1.00% max      

Vanadium

0.20 – 0.50%

Manganese

1.00% max      

Iron

Balance

Physical Properties of 422 Stainless Steel

Density

Heat Treatment

Hardening

0.280 lb/cubic inch

Heat treatment is sensitive as the alloy is very susceptible to cracking

In the annealed condition, typical hardness is Rc 21/25.

In the quenched and tempered condition, hardness is typically Rc 45/50.

Mechanical Proporties of 422 stainless steel

422 bar is readily machinable in the annealed condition with machining characteristics similar to those of alloy 420 stainless steel.


Return to top