+44 28 9181 7919

X750 Sheet Stock, Coil AMS 5598, AMS 5542 - Inconel® Alloy Equivalent


Inconel Alloy® X750 is a nickel-chromium austenitic alloy similar to Alloy 600 but made precipitation-hardenable by additions of aluminum and titanium. It has good resistance to corrosion and oxidation along with high tensile and creep-rupture properties at temperatures to 1300°F (700°C).  This material has excellent relaxation resistance and is non-magnetic. It has good elevated temperature strength properties to 1300ºF (700°C) and oxidation resistance to 1800ºF (983˚C). Alloy X750 is resistant to a wide variety of industrial corrosives under both oxidizing and reducing conditions. This alloy also has excellent resistance to chloride stress corrosion cracking in the fully age hardened condition.

Standard Inventory Specifications 

  • UNS N07750
  • AMS 5598
  • AMS 5542
  • ASTM B 637
  • ASME SB 637
  • W.Nr 2.4669
  • PWA-LCS
  • GE-S400/1000
  • RR SABRe Edition 2
  • DFARS Compliant

Common Trade Names

  • ATI X-750 (™ Allegheny Technologies)
  • Inconel Alloy X-750  (® Special Metals)

Common Applications of Alloy X750

  • Structural members in hot sections of gas turbines such as discs, thrust reversers, and ducts
  • Aircraft structures
  • Rocket engines
  • Nuclear reactors
  • Heat treat fixtures
  • Cryogenic vessels, springs, and fasteners
  • Wire formulation with heat temper used in springs at elevated temperatures

Inventory Size Range

  • Sheet : 0.023" - 0.075" 

All of our Alloy X750 nickel sheet and coil is ordered to specific decimal thicknesses.  Alloy X750 coil can also be slit to your desired width. Please contact us for more details.

The technical data provided is for information only and not for design purposes. It is not warranted or guaranteed.

Alloy X750 Chemical Composition

 

Ni(+Co)

Cr

Fe

Ti

Al

No(+Ta)

Min

70.00

14.0

5.0

2.25

0.40

0.70

Max

--

17.0

9.0

2.75

1.00

1.20

 

 

Si

S

Cu

C

Co

Min

--

---

--

--

--

Max

0.50

0.01

0.50

0.08

1.00

 

Alloy X750 Physical Properties

   

Density

0.298 lb/inᶟ, 8.26 g/cmᶟ

Melting Range

2540-2600°F, 1395-1425°C

Curie Temperature

-225°F as hot-rolled

       -193 triple-heat-treated (2100°F/2 hr, A.C., +1500°F/24 hr, A.C. + 1300°F/20 hr, A.C.)             

Magnetic Permeability

70°F, 200H, as hot rolled 1.0020

1.0035 triple-heat-treated (2100°F/2 hr, A.C., +1500°F/24 hr, A.C., +1300°F/20 hr, A.C.)

Emissivity  Oxidized Surface

600°F  0.895, 2000°F  0.925

Linear Contraction During Precipitation Treatment

1300°F/20 hr), in/in  Hot-rolled 0.00044, 20% Cold-rolled 0.00052, Annealed 0.00026

Mechanical Properties and Yield Strength of Alloy X750

Minimum Specified Properties

Ultimate Tensile Strength, ksi

120

.02% Yield Strength, ksi

60

Elongation, %

30


Return to top