718 Cold Reduced Nickel Bar - AMS 5962


Alloy 718 cold reduced nickel bar is a precipitation hardening nickel-chromium alloy containing significant amounts of columbium, aluminum, molybdenum and titanium. The alloy is cold worked after solution annealing and is typically used for high strength fasteners requiring a room temperature minimum tensile strength of 220 ksi after precipitation hardening. It is typically used at temperatures up to 900° F. This grade has oxidation resistance up to 1800° F. Alloy 718 cold reduced nickel is multiple melted usually with either a vacuum induction melt (VIM) followed by a vacuum arc remelt (VAR), or a vacuum induction melt (VIM) followed by an electroslag remelt (ESR).

Standard Inventory Specifications

  • Cold Reduced
  • AMS 5962
  • AMS 5662 (Chem only)
  • B50TF15 (Chem only)
  • C50TF13 (Chem only)
  • Hi Shear 156 (Chem only) Type 2*
  • SPS M 637
  • MS 319
  • AIC MS 110
  • VMS 110
  • DMS 2209
  • PWA LCS
  • GE S400/S1000
  • RR SABRe Edition 2
  • DFARS compliant

Common Trade Names

  • Nickel 718 Cold Reduced, Alloy 718 Cold Reduced, Inconel® 718 Cold Reduced

Industry Applications

  • Aerospace
  • Fasteners

Inventory Size Range

  • Bar : 0.260" - 1.6235"

Standard Inventory Lengths: 10-12 feet rl's. 

Please contact us for more details.

The technical data provided is for information only and not for design purposes. It is not warranted or guaranteed.

* INCONEL and INCOLOY are trademarks of the Special Metals Corporation group of companies. 

Chemical Composition of 718 Cold Reduced Nickel

Element

Percent by Weight

Nickel

50.0/55.0%

Aluminum

0.20/0.80%

Silicon

0.35% max

Chromium

17.0/21.0%

Cobalt

1.00% max

Phosphorus

0.015% max

Columbium

4.75/5.50%

Boron

0.006% max

Sulfur

0.15% max

Molybdenum

2.80/3.30%

Carbon

0.08% max

Copper

0.30% max

Titanium

0.65/1.15%

Manganese

0.35% max

Iron

Balance

Mechanical Properties of 718 Cold Reduced Nickel

 

 

Tensile Strength    

160 ksi minimum

Yield Strength        

120 ksi minimum

Elongation (4D)

12% minimum

Hardness  

Rc32 minimum

Reduction of Area

18% minimum

 


Return to top

Nominal Composition

  • Nickel - 50.0/55.0%
  • Aluminum - 0.20/0.80%
  • Silicon - 0.35% max
  • Chromium - 17.0/21.0%
  • Cobalt - 1.00% max
  • Phosphorus - 0.015% max
  • Columbium - 4.75/5.50%
  • Boron - 0.006% max
  • Sulfur - 0.15% max
  • Molybdenum - 2.80/3.30%
  • Carbon - 0.08% max
  • Copper - 0.30% max
  • Titanium - 0.65/1.15%
  • Manganese - 0.35% max
  • Iron Balance

718 cold reduced nickel alloy is typically used at temperatures up to 900° F. This grade has oxidation resistance up to 1800° F. Alloy 718 cold reduced nickel is multiple melted usually with either a vacuum induction melt (VIM) followed by a vacuum arc remelt (VAR), or a vacuum induction melt (VIM) followed by an electroslag remelt (ESR).

  • Tensile strength - 160 ksi min
  • Yield strength - 120 ksi min
  • Elongation (in 4D) - 12% min
  • Reduction of Area - 18% min
  • Hardness - Rc32 min